Open 12W in the appJump to the cards

How to drill 12W

  1. Pick one deck below and cover the answers with your hand or a sheet of paper.
  2. Engineer decks mix materials, measurements and safety rules. Keep scrap paper close and work out any numbers before you check the answer.
  3. When a deck feels easy, open 12W in the app and choose Practice test. It asks multiple-choice questions built from these same cards.

With 243 cards, try about 10 short rounds of 25 cards instead of one long session. One or two rounds a day keeps it fresh.

12W decks on this page

12W – Deep Dive: Duties, Building Layout, Batter Boards & Formwork

Source: DA Pam 611-21 ch. 10C (10-12W, Oct 2026 copy); TM 3-34.47 (Carpentry, 29 Jul 2022). Complements mos-12w-carpentry-masonry; does not repeat those cards. Verify current editions.

12W deep dive: Is 12W an Army Civilian Acquired Skills Program (ACASP) designated MOS?
Yes. MOS 12W is an ACASP designated MOS.
DA Pam 611-21 (ch. 10C, Oct 2026 copy), 10-12W heading
12W deep dive: What civilian experience does DA Pam 611-21 require for 12W ACASP qualification?
A minimum of 2 years experience as an apprenticed member of a recognized United States Carpentry and Masonry association.
DA Pam 611-21 (ch. 10C, Oct 2026 copy), 10-12W b(7)
12W deep dive: Does a Soldier who qualifies for 12W under ACASP have to attend AIT?
No. An Initial Entry Trainee (IET) who qualifies under ACASP will not be required to attend AIT. After Basic Combat Training, the Soldier is processed in accordance with initial assignment instructions.
DA Pam 611-21 (ch. 10C, Oct 2026 copy), 10-12W b(7)(a)
12W deep dive: Who approves and validates 12W ACASP qualification for an Initial Entry Trainee?
The USAES Engineer Personnel Development Office (EPDO).
DA Pam 611-21 (ch. 10C, Oct 2026 copy), 10-12W b(7)(b)
12W deep dive: Besides completing the 12W course, how else can a Soldier meet the formal-training requirement for initial award of MOS 12W?
By meeting the civilian acquired skills criteria in Chapter 9-5 (5)(b) of DA Pam 611-21 and the ACASP qualification criteria in 10-12W paragraph b(7).
DA Pam 611-21 (ch. 10C, Oct 2026 copy), 10-12W b(6)
12W deep dive: What minimum OPAT scores does DA Pam 611-21 list for 12W?
Standing Long Jump 120 cm, seated Power Throw 350 cm, Strength Deadlift 120 pounds, and Interval Aerobic Run 36 shuttles, in Physical Demand Category Moderate (Gold).
DA Pam 611-21 (ch. 10C, Oct 2026 copy), 10-12W b(4)(b)
12W deep dive: Why does DA Pam 611-21 require freedom from vertigo for 12W?
To permit climbing, balancing, and working in high places.
DA Pam 611-21 (ch. 10C, Oct 2026 copy), 10-12W b(5)
12W deep dive: Besides constructing floor, stair, roof, and wall systems, what installation and finishing tasks does a 12W1O perform?
Installs batter boards, suspended ceilings, exterior finishes, interior coverings, floor and wall tiles, and doors and windows; places concrete; applies roof coverings; fabricates joints and splices; erects pre-engineered buildings; prepares material takeoff lists; applies interior trim; identifies building materials; and maintains carpentry and masonry tools.
DA Pam 611-21 (ch. 10C, Oct 2026 copy), 10-12W a(1)
12W deep dive: What emergency skill does DA Pam 611-21 list among 12W1O duties?
Rescuing an electrical shock victim.
DA Pam 611-21 (ch. 10C, Oct 2026 copy), 10-12W a(1)
12W deep dive: What construction and testing duties does a 12W2O perform?
Constructs foundations, constructs overhead forms, and performs slump tests.
DA Pam 611-21 (ch. 10C, Oct 2026 copy), 10-12W a(2)
12W deep dive: What planning, inspection, and safety duties does a 12W2O perform?
Coordinates construction planning and advises on carpentry and masonry construction; directs operational maintenance on assigned equipment; inspects carpentry and masonry components for proper installation; and ensures employment of proper safety procedures.
DA Pam 611-21 (ch. 10C, Oct 2026 copy), 10-12W a(2)
12W deep dive: Where should a line level be placed for the greatest accuracy when leveling two points?
Halfway between the points to be leveled, hung from a taut line.
TM 3-34.47 (29 Jul 2022), para 4-1
12W deep dive: What are batter boards?
A temporary framework used to assist in locating corners when laying out a foundation. Posts are 2 x 4 or 4 x 4 material, corner stakes are 2 x 2s, and the boards are 1 x 4 or 1 x 6 pieces.
TM 3-34.47 (29 Jul 2022), para 4-10
12W deep dive: Why are batter boards set up outside the corner stakes?
Excavating for a foundation will disturb the corner stakes, so batter boards are set up outside that boundary to preserve definite and accurate building lines. Heavy cord or fine wire is stretched from one batter board to another to mark these lines.
TM 3-34.47 (29 Jul 2022), para 4-11
12W deep dive: How far outside the stakes are batter boards erected?
Right-angle batter boards are erected 3 or 4 feet outside of each corner stake. Straight batter boards are erected 3 or 4 feet outside of the line stakes.
TM 3-34.47 (29 Jul 2022), para 4-12
12W deep dive: At what height are right-angle batter boards set, and how are the lines held in place?
At the exact height of the top of the foundation. Angle saw cuts or nails in the tops of the boards hold the lines; separate cuts or nails may be used for the building line, foundation line, footing line, and excavation lines so the lines can be removed and replaced correctly.
TM 3-34.47 (29 Jul 2022), para 4-13
12W deep dive: What two methods are commonly used to square extended building lines?
The 6-8-10 method and the diagonal method.
TM 3-34.47 (29 Jul 2022), para 4-17
12W deep dive: How is the 6-8-10 method used to square building lines, and what is the minimum starting measurement?
Measure 6 feet along one line and 8 feet along the other, then adjust the lines until the distance between those points equals 10 feet. Multiples such as 12-16-20 may be used for large layouts. For accuracy, never start with a measurement of less than 6 feet.
TM 3-34.47 (29 Jul 2022), para 4-18
12W deep dive: How does the diagonal method prove that a rectangular layout is square?
Lines cutting the rectangle from opposing corners form two triangles. If the rectangle is perfect, those diagonal lines are equal in length and the corners are square. If they are not equal, adjust the corners by moving the lines right or left until the diagonals are equal.
TM 3-34.47 (29 Jul 2022), para 4-19
12W deep dive: When are wall foundations used, and what reinforcement rule applies to concrete foundation walls?
Wall foundations are solid for their total length and are usually used when heavy loads are to be carried or the earth has low supporting strength. Steel-rod reinforcements should be used in all concrete walls. Because of the time, labor, and material required, this type of wall is used in the theater of operations only when other types cannot be used.
TM 3-34.47 (29 Jul 2022), para 4-21
12W deep dive: When must mortar be used in rubble stone masonry?
Rubble masonry may be laid up with or without mortar, but mortar must be used if strength and stability are desired. In military construction it is used when form lumber for masonry units is not available.
TM 3-34.47 (29 Jul 2022), para 4-22
12W deep dive: How far apart are column or post foundations usually spaced, and when must wood posts be braced?
In most cases the posts or columns are spaced 6 to 10 feet apart. When wood posts extend 3 feet or more above the ground, braces are necessary.
TM 3-34.47 (29 Jul 2022), para 4-25
12W deep dive: Why must concrete forms be tight, rigid, and strong?
If forms are not tight, loss of concrete may cause a honeycomb effect, or loss of water may cause sand-streaking. The forms must be braced enough to stay in alignment. Special care is needed when bracing and tying down forms for retainer walls and the first pour for walls and columns, because the concrete tends to lift the form above its proper elevation.
TM 3-34.47 (29 Jul 2022), para 5-1
12W deep dive: Why should form lumber be only partially seasoned, not kiln-dried?
Kiln-dried lumber tends to swell when soaked with water, and swelling may cause bulging and distortion. If green lumber is used, allow for shrinkage, or keep it wet until the concrete is in place. Softwoods (pine, fir, and spruce) are the most economical.
TM 3-34.47 (29 Jul 2022), para 5-4
12W deep dive: What form-work safety precautions does TM 3-34.47 list after discussing plywood forms?
Watch for protruding nails (the principal cause of accidents on form work); inspect tools frequently; place mud sills under shoring that rests on the ground; protect all men on scaffolds and on the ground; do not raise large form panels in heavy gusts of wind; and brace all shoring securely to prevent collapse of form work.
TM 3-34.47 (29 Jul 2022), caution after para 5-7
12W deep dive: What lumber should be used on the concrete face of a wood form, and which joint is most watertight?
Wood coming in contact with concrete should be surfaced (smooth) on the side toward the concrete and on both edges. Edges may be square, shiplap, or tongue-and-groove. Tongue-and-groove lumber makes a more watertight joint, which reduces warping.
TM 3-34.47 (29 Jul 2022), para 5-5
12W deep dive: What plywood is used for wall and floor forms?
Plywood used for forms should be made with waterproof glue and marked for use in concrete forms. It is warp-resistant and can be used more often than other lumber.
TM 3-34.47 (29 Jul 2022), para 5-6
12W deep dive: How should form nails be driven when footing-form panels are held in place until the tie wire is installed?
Use form nails, and drive them only part way from the outside so they can be easily removed.
TM 3-34.47 (29 Jul 2022), para 5-10
12W deep dive: When must reinforcing bars be placed in a footing form relative to the tie wire, and how large may the wire holes be?
Reinforcing bars must be placed before the wire is installed. Wire holes on each side of the cleat should be less than 1 inch in diameter to prevent mortar leaks. Tie wires are wrapped around the center cleats.
TM 3-34.47 (29 Jul 2022), para 5-11
12W deep dive: How are forms for footings 4 feet square or larger kept from spreading?
Stakes are driven, and 1 x 6 boards are nailed across the top of the form. If the footings are less than 1 foot deep and 2 feet square, forms can be built of 1-inch sheathing without cleats.
TM 3-34.47 (29 Jul 2022), para 5-12
12W deep dive: How long may prefabricated wall-form panels be?
No more than 10 feet long so they can be easily handled.
TM 3-34.47 (29 Jul 2022), para 5-16
12W deep dive: What sheathing is normally used on a concrete wall form, and why must it be watertight?
It is normally 1-inch (3/4-inch dressed) tongue-and-groove lumber or 3/4-inch plywood. Concrete is plastic when placed, so sheathing should be watertight, and it must be reinforced to prevent bulging from the weight of the concrete.
TM 3-34.47 (29 Jul 2022), para 5-17
12W deep dive: When do vertical form studs need reinforcing?
Studs are generally made from 2 x 4 lumber and also require reinforcing when they extend more than 4 feet.
TM 3-34.47 (29 Jul 2022), para 5-18
12W deep dive: What do double wales do on a wall form?
They reinforce the wall form, tie wall panels together, and keep them in a straight line. They run horizontally and are lapped at the corners.
TM 3-34.47 (29 Jul 2022), para 5-19
12W deep dive: What is the usual angle of a wall-form brace, and do braces count in form design strength?
The most common brace uses a horizontal member and a diagonal member nailed to a stake and to the stud or wale. The diagonal should make a 30° angle with the horizontal member. Braces are not part of the form design and are not considered as providing additional strength.
TM 3-34.47 (29 Jul 2022), para 5-20
12W deep dive: How are spreaders sized and held in a wall form, and when are they removed?
Spreaders are cut to the same length as the wall thickness, placed between the two sheathing surfaces near each tie wire, and held by friction, not nails. They are removed as the forms are filled so they will not become embedded as the concrete hardens.
TM 3-34.47 (29 Jul 2022), paras 5-22 and 5-23
12W deep dive: How are tie wires installed in wall forms, and what wire may be used in an emergency?
Double strands are always used. The wire should be No. 8 or 9 gauge, black, annealed iron wire; barbed wire may be used in an emergency. Tie spacing should be the same as the stud placing, but never more than 3 feet. Wire ties should be used only for low walls or when tie rods are not available.
TM 3-34.47 (29 Jul 2022), para 5-24
12W deep dive: After a form with a tie-rod and spreader combination is removed, what is done with the rods?
Each rod is broken off at the notch. If appearance is important, the holes should be filled with a mortar mix.
TM 3-34.47 (29 Jul 2022), para 5-25
12W deep dive: Why does a column form have a cleanout hole, and when is the column form erected?
The form should have a cleanout hole in the bottom to help remove debris. The lumber removed to make the hole should be nailed to the form so it can be replaced before the concrete is positioned. The column form is erected after the steel reinforcement is assembled and tied to dowels in the footing.
TM 3-34.47 (29 Jul 2022), para 5-28
12W deep dive: Do beam forms take much bursting pressure, and how must they be supported?
Beam forms receive little bursting pressure but must be shored at close intervals to prevent sagging.
TM 3-34.47 (29 Jul 2022), para 5-29
12W deep dive: How wide may stair forms be built with the method in TM 3-34.47, and what material is used on the underside of the steps?
Up to 3 feet in width. The underside of the steps should be 1-inch tongue-and-groove sheathing, and the platform should extend 12 inches beyond each side of the stairs to support stringer bracing blocks. The face of the riser should be 2-inch material, beveled.
TM 3-34.47 (29 Jul 2022), para 5-33
12W deep dive: How are wood forms treated before concrete is placed so the concrete will not stick?
Forms are treated with oil or another coating. The oil should penetrate the wood to prevent water absorption; a light-bodied petroleum oil will do. On plywood, shellac is more effective than oil. If forms will be reused, painting helps preserve the wood.
TM 3-34.47 (29 Jul 2022), para 5-34
12W deep dive: What may be used if form oil is not available?
Wetting with water may be substituted in an emergency to prevent sticking.
TM 3-34.47 (29 Jul 2022), para 5-35
12W deep dive: How should forms be wedged and stripped to avoid breaking the edges of the concrete?
Use wood wedges rather than a pinchbar or other metal tool. Do not jerk forms off after wedging has been started at one end. Forms to be reused should be cleaned and oiled immediately, and nails should be removed as forms are stripped.
TM 3-34.47 (29 Jul 2022), para 5-36
12W deep dive: What safety rules apply when stripping concrete forms?
Permit only workmen doing the stripping in the immediate area. Do not remove forms until the concrete has set. Pile stripped forms immediately to avoid congestion, exposed nails, and other hazards.
TM 3-34.47 (29 Jul 2022), caution after para 5-36
12W deep dive: What are the three principal types of framing for light structures?
Western, balloon, and braced.
TM 3-34.47 (29 Jul 2022), para 6-2
12W deep dive: Why is western or platform framing preferred for one-story military buildings?
It is used extensively in military construction. It has boxed-sill construction at each floor line and uses cross bridging between joists and bridging between studs. It is preferred for one-story structures because it permits both bearing and nonbearing walls (supported by the joist) to settle uniformly.
TM 3-34.47 (29 Jul 2022), para 6-5
12W deep dive: How does balloon framing differ from braced framing in a multistory building?
In balloon framing the studs run the full length, from sill to rafters. Second-floor joists customarily rest on a 1- x 4-inch ribbon set into the studs. The balloon frame is less rigid than a braced frame.
TM 3-34.47 (29 Jul 2022), para 6-6
12W deep dive: How is a braced frame built, and why is it more rigid than a balloon frame?
Exterior studs extend only between floors and are topped by girts (usually 4 x 6 inches) that form a sill for the joists of the next floor. Sills and corner posts are customarily 4 x 6 inches; corner posts extend from sill to plate. Knee braces, usually 2 x 4 inches, are placed diagonally against each side of the corner posts.
TM 3-34.47 (29 Jul 2022), para 6-7
12W deep dive: When is heavy framing used, and how large are the members?
Heavy-frame buildings are more permanent and are normally used for warehouses and shops. Heavy framing is seldom used in theater-of-operations construction. Members are at least 6 inches in dimension (timber construction).
TM 3-34.47 (29 Jul 2022), para 6-8
12W deep dive: Where do weak points usually occur in a timber structure?
At the connections (joints and splices) between pieces of lumber. Those connections can be structurally sound if done correctly; weak points are usually a sign of poor workmanship.
TM 3-34.47 (29 Jul 2022), para 6-10
12W deep dive: What is the difference between a joint and a splice?
Joints connect two pieces of timber that come together at an angle. The types most commonly used in carpentry are butt joints and lap joints. Splices connect two or more pieces of material that extend in the same line.
TM 3-34.47 (29 Jul 2022), paras 6-11 and 6-19
12W deep dive: Which carpentry joint is weakest, and which is strongest?
A butt joint is the weakest type of joint, especially if it is made of only two pieces of wood, because the end grain is the weakest part of a piece of wood when used in joints. The lap joint is the strongest joint.
TM 3-34.47 (29 Jul 2022), paras 6-13 and 6-16
12W deep dive: What kind of splice should be used for vertical supports, for trusses or joists, and for girders or beams?
Vertical supports (longitudinal stress) require splices that resist compression. Trusses, braces, and joists (transverse and angular stress) require splices that resist tension. Horizontal supports such as girders or beams require splices that resist bending tension and compression. Splices for resisting compression are usually worthless for resisting tension or bending.
TM 3-34.47 (29 Jul 2022), paras 6-19 and 6-20
12W deep dive: What are fishplates and scabs?
Metal plates used as supports in a butt splice are called fishplates. Wood plates are called scabs and are fastened with bolts or screws. If nails are used with scabs, they are staggered and driven at an angle away from the splice; too many nails, or nails that are too large, will weaken a splice.
TM 3-34.47 (29 Jul 2022), para 6-20
12W deep dive: What is a sill, and how is air kept from entering under it?
The sill is the foundation that supports a building and is the first part of a building to be set in place. It rests directly on the foundation posts or on the ground. To prevent air from entering the building, spread a thin bed of mortar on top of the foundation wall, which also provides a solid base for the sill. A fiberglass sill sealer may also be used.
TM 3-34.47 (29 Jul 2022), para 6-25
12W deep dive: Which sill is commonly used with platform framing?
Box sills, which may be used with or without the sill plate. Platform framing is the most common type of framing.
TM 3-34.47 (29 Jul 2022), para 6-26
12W deep dive: What is a girder, and how much end bearing should a wood girder have?
A girder is a large beam that supports other smaller beams or joists when the distance between two outside walls is too great to be spanned by a single joist. The ends of wood girders should bear at least 4 inches on posts. Precautions must be taken to avoid or counteract any future settling or shrinking, which would distort the building.
TM 3-34.47 (29 Jul 2022), paras 6-32 and 6-34
12W deep dive: To increase a girder's carrying capacity, is it better to add width or depth?
Within limits, it is better to increase the girder's depth than its width. When the depth is doubled, the safe load increases four times. For example, a girder 3 inches wide and 12 inches deep will carry four times as much weight as a girder 3 inches wide and 6 inches deep. A girder should be just large enough to support an ordinary load; any size larger wastes material.
TM 3-34.47 (29 Jul 2022), para 6-38
12W deep dive: What dead-load allowances does TM 3-34.47 use for a light-frame building similar to an ordinary frame house?
Allow 10 pounds per square foot for an average subfloor, finish floor, and joists without basement plaster; add 10 pounds per square foot if the basement ceiling is plastered; allow 20 pounds for ceiling plaster and joists if the attic is unfloored when girders or bearing partitions support the first-floor partition; and allow an additional 10 pounds per square foot if the attic is floored and used for storage.
TM 3-34.47 (29 Jul 2022), para 6-47
12W deep dive: What live-load allowances does TM 3-34.47 list for floors used for living purposes?
Allow 30 pounds per square foot for live load on floors used for living purposes. If the attic is floored and used for light storage, allow an additional 20 pounds per square foot. Snow on the roof is also part of the live load. Local building specifications usually govern the allowance.
TM 3-34.47 (29 Jul 2022), para 6-48
12W deep dive: How thick are floor joists, how far apart are they spaced, and which way is the crown placed?
Joists are usually 2 or 3 inches thick and are spaced 16 or 24 inches apart, center to center (sometimes 12 inches, but heavier joists should then be used). Joists as small as 2 x 6 are too small for floors with spans over 10 feet, but are frequently used for ceiling joists. The joist is always placed crown up to counteract the weight; in most cases there will be no sag below a straight line.
TM 3-34.47 (29 Jul 2022), paras 6-67, 6-68, and 6-71
12W deep dive: Why are floor frames bridged, and which kind of bridging is used most often?
Joists tend to twist, especially over a long span. Bridging stiffens the floor frame, prevents unequal deflection, and lets an overloaded joist get help from the joists on either side. The three kinds are solid (horizontal) bridging, cross bridging, and compression bridging. Cross bridging is used most often; it is made of diagonally cut 1 x 3 or 2 x 3 pieces and requires less time than horizontal bridging.
TM 3-34.47 (29 Jul 2022), paras 6-77 and 6-78
12W deep dive: When should the bottom ends of cross bridging be nailed, and how many lines of bridging are required?
Nail the tops first and leave the bottoms free until the subfloor is laid, so the joists can adjust and the bridging does not push the joists up and make the floor uneven. Then nail the bottom ends, forming a continuous truss. Use one line of bridging on joists more than 8 feet long, and two lines on joists more than 16 feet long.
TM 3-34.47 (29 Jul 2022), paras 6-79 and 6-80
12W deep dive: How is a floor opening for a stairwell, ventilator, or chimney framed?
With a combination of headers and trimmers. Headers run at right angles to the joists and are doubled. Trimmers run parallel to the joists and are actually doubled joists. The shorter joists framed to the headers are called tail beams, tail joists, or header joists.
TM 3-34.47 (29 Jul 2022), para 6-81
12W deep dive: How is subflooring laid in theater-of-operations construction?
If included in the plans, the subfloor is laid diagonally on the joist framework and nailed with 8d to 10d nails. Boards 8 inches wide or more should have at least three nails per joist. The subfloor is normally laid before the walls are framed so it can be walked on while the walls are being framed.
TM 3-34.47 (29 Jul 2022), para 6-84
12W deep dive: How much vent area is required in a building?
Place one square foot of vent for each 150 square feet of floor space without soffit vents, and for each 300 square feet of floor space with soffit vents. The minimum net open area should be 1/4 square inch per square foot of ceiling area.
TM 3-34.47 (29 Jul 2022), para 6-149
12W deep dive: Why must crawl spaces be ventilated, and what louver area is required under the floor?
Air circulation under the flooring prevents excessive condensation, which causes warping, swelling, twisting, and rotting of the lumber. Foundation louvers should be figured on the same basis as upper-structure louvers: 1/4 square inch for each square foot of under-floor space. A good foundation vent should have a copper or bronze screen and adjustable shutters.
TM 3-34.47 (29 Jul 2022), para 6-151
12W deep dive: How many stringers are used on a stair more than 36 inches wide, and what is the usual stringer size?
There are usually three stringers if the stairs are more than 36 inches wide—one at each outer edge and one at the center. Stringers (or carriages) are 2 to 3 inches thick and 8 or more inches wide, and they are cut to form the step of the stairs.
TM 3-34.47 (29 Jul 2022), paras 6-152 and 6-153
12W deep dive: What rules of thumb check riser and tread dimensions, and how is tread width figured?
Riser height plus tread width should be between 17 and 19 inches, and riser height times tread width should be between 70 and 75 inches. There is always one more riser than tread, so tread width is the run of the stairs divided by the number of risers less one. These figures will be about 7 and 10 inches, since the ideal run and rise totals 17 inches.
TM 3-34.47 (29 Jul 2022), paras 6-156, 6-157, and 6-158
12W deep dive: What members make up a wall frame, and what do the studs support?
Wall framing consists of studs, diagonal bracing, cripples, trimmers, headers, and fire blocks, supported by the floor sole plate. The studs are the vertical members; they support the top plates and everything above the top plate line, plus the lath, plaster, and insulation on the inside and wall sheathing on the outside.
TM 3-34.47 (29 Jul 2022), para 6-93
12W deep dive: How are stud walls assembled, and what ties the walls together at the top?
Studs are usually closely spaced, slender, 2 x 4 vertical members. Their ends bear on a long horizontal bottom plate or sole plate, and their tops are capped with a top plate. Double top plates are used to tie walls and partitions together. The bearing strength of stud walls is determined by the strength of the studs.
TM 3-34.47 (29 Jul 2022), para 6-94
12W deep dive: What is the difference between bearing and nonbearing partition walls?
A bearing partition supports ceiling joists. A nonbearing partition supports only itself and may be put in at any time after the other framework is installed; only one cap or plate is used. A sole plate should be used in every case, because it helps distribute the load over a larger area.
TM 3-34.47 (29 Jul 2022), para 6-96
12W deep dive: What does the top plate do, and what is the sole plate?
The top plate ties the studding together at the top, forms a finish for the walls, and supports the lower ends of the roof rafters. It is made of one or two pieces of framing lumber the same size as the studs. The sole or sole plate is a 2 x 4, or a piece the same thickness as the wall, laid horizontally to carry the bottom end of the studs.
TM 3-34.47 (29 Jul 2022), paras 6-107 and 6-109
12W deep dive: How are frame walls bridged, and which method is more effective?
Frame walls are usually bridged to make them more sturdy, either horizontally or diagonally. Horizontal bridging is nailed between the studs halfway between the sole and top plates and helps straighten the studs. Diagonal bridging is nailed at an angle and is more effective because it forms a continuous truss and keeps the walls from sagging. Interior partitions and exterior walls should be bridged alike whenever possible.
TM 3-34.47 (29 Jul 2022), paras 6-110, 6-111, and 6-112
12W deep dive: What must a theater-of-operations roof do, and what factors decide the roof type?
The roof's main purpose is to keep out the rain, cold, or heat. It must be strong enough to withstand high winds, sloped to shed water, and, in areas of heavy snow, constructed more rigidly to bear the extra weight. Roofs for the theater of operations are chosen to suit the building, the climate, the estimated length of time the building will be used, and the material, time, and skill required for construction.
TM 3-34.47 (29 Jul 2022), chapter 7 introduction and para 7-1
12W deep dive: How are rafters sized, spaced, and fastened?
Rafters make up the main framework of all roofs. They are inclined members spaced from 16 to 48 inches apart, and they vary in size depending on length and spacing. The tops are fastened to the ridge or another rafter; they rest on the top wall plate. Rafters are nailed to the plate, not framed into it. They may extend a short distance beyond the wall to form the eaves and protect the sides of the building.
TM 3-34.47 (29 Jul 2022), paras 7-3 and 7-4
12W deep dive: What is the cut, span, rise, and line length of a roof?
The span is the shortest distance between the two opposite rafters' seats. The rise of a rafter is the vertical (or plumb) distance that a rafter extends upward from the plate. The cut of a roof is the rise over the run (such as a 4/12 roof) or the pitch of the roof. Line length is the hypotenuse of a triangle whose base is the run and whose altitude is the total rise. The square of the hypotenuse of a right triangle equals the sum of the squares of the two sides.
TM 3-34.47 (29 Jul 2022), para 7-4
12W deep dive: What are the four types of rafters?
Common rafters extend at right angles from the plate line to the roof ridge and are used as the basis for laying out other types. Hip rafters extend diagonally from the corner of the plate to the ridge. Valley rafters extend from the plate to the ridge along the lines where two roofs intersect. Jack rafters are a type of common rafter: a hip jack runs from the plate to the hip rafter, a valley jack from the ridge to the valley rafter, and a cripple jack is placed between a hip rafter and a valley rafter and touches neither the ridge nor the rafter plate.
TM 3-34.47 (29 Jul 2022), paras 7-5 through 7-9
12W deep dive: What is a collar tie, and how often must collar ties be placed?
A collar tie or beam is a piece of stock (usually 1 x 4, 1 x 6, 1 x 8, or 2 x 4) fastened horizontally to a pair of rafters between the plate and the ridge. It keeps the building from spreading. Most codes and specifications require them to be 5 feet apart or every third rafter, whichever is less. This bracing is used on small roofs where no ceiling joists are used and the building is not wide enough to require a truss.
TM 3-34.47 (29 Jul 2022), para 7-10
12W deep dive: After two rafters have been cut, what should be done before cutting the rest?
When laying off rafters by any method, recheck the work carefully. When two rafters have been cut, it is best to put them in place to see if they fit. Minor adjustments may be made at this time without serious damage or waste of material.
TM 3-34.47 (29 Jul 2022), para 7-14 note
12W deep dive: What pitch does a rafter have with a run of 12 and a rise of 4, 6, or 12?
A rafter with a run of 12 and a rise of 4 has a 1/6 pitch, 12 and 6 has a 1/4 pitch, and 12 and 12 has a 1/2 pitch.
TM 3-34.47 (29 Jul 2022), para 7-22
12W deep dive: What is a truss, and which types are most commonly used in building construction?
A truss is a framed or jointed structure of straight members connected only at their intersections so that if loads are applied at those intersections, the stress in each member is in the direction of its length. Straight, sound timber should be used. The Howe and Fink trusses are most commonly used. Trusses are used for large spans to give wide, unobstructed floor space, such as in shops and hangars.
TM 3-34.47 (29 Jul 2022), paras 7-25 and 7-26
12W deep dive: What are purlins used for in roof construction?
Purlins support corrugated sheet metal, if it is used, or the sheathing of roofs framed with trusses. In small roofs, purlins are inserted between the rafters and nailed through the rafters. In large buildings with heavy trusses, the purlins are continuous members that rest on the trusses and support the sheathing. In small buildings such as barracks, mess halls, and small warehouses, 2 x 4s are used for purlins, with the narrow side up.
TM 3-34.47 (29 Jul 2022), para 7-29
12W deep dive: Why is flashing installed, and which roof areas are most subject to leakage?
Places especially susceptible to leakage in roofs and outside walls are made watertight by flashing, which is sheets of material used to cover those places. Ridge lines and hip lines naturally tend to shed water and are only moderately subject to leakage. Valleys are more subject to leakage because water gathers in them.
TM 3-34.47 (29 Jul 2022), paras 7-55, 7-56, and 7-57

12W – Deep Dive: Concrete Mix, Slump Test, Form Safety & Masonry

Source: TM 3-34.44 (Concrete and Masonry, 23 Jul 2012 incl. C1, 2 Sep 2021). Complements mos-12w-carpentry-masonry and mos-12w-3; does not repeat those cards. Verify current editions.

12W deep dive: What is concrete, and what causes it to harden?
Concrete is a mixture of aggregate, and often controlled amounts of entrained air, held together by a hardened paste made from cement and water. A chemical reaction between the portland cement and water—not drying of the mixture—causes concrete to harden to a stone-like condition. This reaction is called hydration and gives off heat, known as the heat of hydration. Because hydration—not air drying—hardens concrete, freshly placed concrete submerged underwater will harden.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 1-1
12W deep dive: How does the amount of water in a mix affect concrete strength?
The basic ratio of cement to water determines the concrete's strength; generally, the less water in the mix, the stronger, more durable, and more watertight the concrete. Too much water dilutes the cement paste (binder), resulting in weak and porous concrete. Unless tests or experience show that a particular water source is satisfactory, water should be free from acids, alkalis, oils, and organic impurities.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 1-3
12W deep dive: How much of normal concrete is aggregate, and how does mortar differ from concrete?
Inert filler materials (usually sand and stone or gravel) make up between 60 and 80 percent of the volume of normal concrete. When cement is mixed with water and aggregates passing the number 4 sieve, the product is mortar, stucco, or cement plaster. When cement is mixed with coarse aggregate of more than 1/4 inch plus fine aggregate and water, the product is concrete.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 1-4
12W deep dive: How is portland cement measured, and how much does a standard sack weigh?
The unit of measure for concrete is the cubic foot. A standard sack of portland cement weighs 94 pounds and equals 1 loose cubic foot. Fine and coarse aggregates are measured by loose volume, and water is measured by the gallon. Concrete is usually referred to by cubic yards.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 1-14
12W deep dive: What is workability, and how is consistency measured?
Workability is the relative ease or difficulty of placing and consolidating concrete in the form. One characteristic of workability is consistency, which is measured by the slump test. A very stiff mix has a low slump and is desirable for many uses, although it is difficult to place in heavily reinforced sections. A more fluid mix is necessary when placing concrete around reinforcing steel.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 1-16
12W deep dive: How far may plastic concrete drop in free fall?
Plastic concrete should not drop (free fall) more than 3 to 5 feet, nor be transported over long distances without proper agitation, so that segregation is kept to a minimum.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 1-17
12W deep dive: How much water does a sack of cement need for hydration, and what W/C range is used in economical mixes?
A sack of cement requires about 2 1/2 gallons of water for hydration. Additional water allows for workability, but too much water (a high water-cement [W/C] ratio) reduces the concrete's strength. The amount of water in economical concrete mixes ranges from 4 gallons minimum to 7 gallons maximum per sack.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 1-20
12W deep dive: What Corps of Engineers watertightness limits apply to mixing water per sack of cement?
For concrete exposed to fresh water, the maximum is 5.5 gallons per sack of cement (W/C = 0.48). For concrete exposed to saltwater, the maximum is 5 gallons per sack (W/C = 0.44). The watertightness of air-entrained concrete is superior to that of nonair-entrained concrete. As the W/C ratio increases, durability decreases.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), paras 1-21 and 1-22
12W deep dive: What is Type I portland cement used for, and when does it reach design strength?
Type I is a general-purpose cement for concrete that does not require the special properties of the other types. It is intended for concrete that is not subjected to a sulfate attack or when the heat of hydration will not cause a minimum temperature rise. It is used in pavement and sidewalk construction and in reinforced concrete buildings, bridges, railways, tanks, reservoirs, sewers, culverts, water pipes, and masonry units. Type I cement will reach its design strength in 28 days and is more available than other types.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 2-4
12W deep dive: What is Type II portland cement used for, and when does it reach design strength?
Type II cement is modified to resist a moderate sulfate attack. It usually generates less heat of hydration and at a slower rate than Type I. Typical applications include drainage structures where sulfate concentrations in the soil or ground water are higher than normal but not severe. Type II cement will reach its design strength in 45 days.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 2-5
12W deep dive: What is Type III portland cement used for, and what caution applies to large members?
Type III is a high-early-strength cement that produces design strengths at an early age, usually seven days or less. It has a higher heat of hydration and is ground finer than Type I. It permits fast form removal and, in cold weather, reduces the period of protection against low temperatures. Use it cautiously in concrete structures having a minimum dimension of 2 1/2 feet or more, because the high heat of hydration can cause shrinkage cracking.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 2-6
12W deep dive: What are Type IV and Type V portland cements used for, and when do they reach design strength?
Type IV has a low heat of hydration and is used primarily in very large concrete structures, such as gravity dams, where the temperature rise from the heat of hydration could damage the structure; it reaches design strength in 90 days. Type V is sulfate-resistant cement used mainly where the concrete is subject to severe sulfate action, such as soil or ground water with a high sulfate content; it reaches design strength in 60 days.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), paras 2-7 and 2-8
12W deep dive: What does air-entraining portland cement do?
Cement types IA, IIA, and IIIA correspond to Types I, II, and III, with small quantities of air-entraining materials interground with the clinker. They produce concrete with improved resistance to freeze-thaw action and to scaling caused by snow and ice removal chemicals. Such concrete contains extremely small, well-distributed, completely separate air bubbles (as many as 3 billion per cubic yard). It is especially useful for sidewalks.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 2-10
12W deep dive: What does the slump test measure, and when should it not be used for comparison?
The slump test measures the consistency of concrete. Do not use it to compare mixes that have different proportions or that contain different sizes of aggregate. When testing different batches of the same mixture, changes in slump indicate changes in materials, mix proportions, or water content.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 3-10
12W deep dive: What slump ranges does TM 3-34.44 recommend for construction when vibration is used?
For reinforced foundation walls and footings, plain footings, caissons and substructure walls, and pavements and slabs: 1 to 3 inches. For beams and reinforced walls, and for building columns: 1 to 4 inches. For mass concrete: 1 to 2 inches. These values may be increased 1 inch for consolidation by methods such as rods and spades.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 3-10 and table 3-4
12W deep dive: What are the dimensions of the slump-test cone, and when does the slump test not apply?
The metal mold is 16-gage galvanized sheet metal shaped like a 12-inch-high truncated cone with an 8-inch-diameter base and a 4-inch-diameter top; both ends are open. The slump test does not apply if the concrete contains aggregates much larger than 2 inches in size. Although not a precise method, it gives sufficiently accurate results in the laboratory and in the field.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), appendix B introduction and para B-2
12W deep dive: What tamping rod is used in the slump test?
The tamping rod is 5/8 inch in diameter, 24 inches long, and has a 1-inch taper at one end terminating in a rounded bullet-nose tip with a radius of about 1/4 inch.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para B-3
12W deep dive: How is the slump-test mold filled and rodded?
Dampen the mold and place it on a flat, moist, nonabsorbent, and firm surface. Fill it immediately with three equal layers. Rotate each scoopful around the top edge as the concrete slides in, so the concrete is distributed symmetrically. Tamp each layer 25 strokes with the tamping rod, distributing the strokes uniformly and penetrating the underlying layer; tamp the bottom layer throughout its depth. After tamping the top layer, strike off the surface with a trowel so the concrete fills the mold exactly, then carefully lift the mold straight up without delay and place it beside the specimen.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para B-5
12W deep dive: How is slump measured, and what should you do if the specimen shears off?
Place the tamping rod across the top of the mold and measure the distance between the bottom of the rod and the displaced original center of the specimen's top surface. If concrete shears off from one side or portion of the mass, disregard the test and make a new test on another portion of the sample. If two consecutive tests show a falling away or shearing off, the concrete probably lacks the plasticity and cohesiveness needed for the slump test to apply.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para B-6
12W deep dive: After the slump is measured, how can you judge whether the mix is well proportioned?
Tap the side of the specimen gently with the tamping rod. A well-proportioned, workable mix will gradually slump (fall or flatten out) but still retain its original consistency, whereas a poor mix will crumble, segregate, and fall apart.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para B-7
12W deep dive: What safety precautions apply when work is progressing on elevated forms?
Take precautions to protect both workers on scaffolds and ground personnel.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 4-62
12W deep dive: Besides watching for protruding nails, what form-construction safety steps does TM 3-34.44 require?
Inspect tools frequently—particularly hammers. Place mudsills under shoring that rests on the ground. Observe the weather, and do not attempt to raise large form panels in heavy wind gusts, either by hand or by crane. Brace all shoring to prevent possible formwork collapse. Protruding nails are the main source of formwork accidents.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 4-63
12W deep dive: What safety rules apply when stripping forms, including tie wires?
Permit only those workers actually stripping forms in the immediate work area. Do not remove forms until the concrete sets. Pile stripped forms immediately to avoid congestion, exposed nails, and other hazards. Take caution when cutting wires under tension to avoid backlash.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 4-64
12W deep dive: What construction deficiencies most often cause wall-form failures?
Failure to control the rate of placing concrete vertically without regard to a drop in temperature; failure to sufficiently nail members; failure to allow for lateral pressures and forces; failure to tighten or secure form ties; use of old, damaged, or weathered form materials; use of undersized form material; and failure to sufficiently allow for eccentric loading due to placement sequences.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 4-66
12W deep dive: What construction deficiencies most often cause overhead slab failures?
Failure to adequately diagonally brace the shores; failure to stabilize soil under mudsills; failure to allow for lateral pressures on formwork; failure to plumb shoring (which induces lateral loading and reduces vertical load capacity); failure to correct deficiencies where locking devices on metal shoring are not locked, inoperative, or missing; failure to prevent vibration from adjacent moving loads or load carriers; and failure to prevent premature removal of supports, especially under long continuous sections.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 4-67
12W deep dive: What safety facilities should be planned during site preparation for concrete work?
Plan and construct overhead canopies and guardrails both to protect personnel from falling debris and to prevent anyone from falling into open excavations. Sites where landslides may occur require additional safety facilities.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 5-11
12W deep dive: How accurately must concrete batch ingredients be measured?
Measure ingredients for each batch within these percentages: cement, 1 percent; aggregate, 2 percent; water, 1 percent; and admixtures, 3 percent. Periodically check equipment for accuracy. Check admixture dispensers daily, particularly for over-dosages, which can cause serious problems in both fresh and hardened concrete. In troop construction, especially in the theater of operations, sacked cement is used almost exclusively.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 5-19
12W deep dive: How is concrete mixed by hand?
Use a clean, even paved surface or a wood platform with tight joints to prevent paste loss. Moisten and level the platform, spread cement over the sand, then spread the coarse aggregate over the cement. Turn the dry materials at least three times until the color is uniform. Add water slowly while turning the mixture again at least three times, or until you obtain the proper consistency. One worker can mix 1 cubic yard by hand in about 1 hour, but that is not economical for batches of more than 1 cubic yard.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 5-20
12W deep dive: When does mixing time start, and what is the minimum mixing time per batch?
Mixing time starts when water runs into the dry mixture, normally during the first quarter of the mixing period. The minimum mixing time per batch is 1 minute unless the batch exceeds 1 cubic yard. Each additional cubic yard, or fraction thereof, requires an additional 15 seconds of mixing time.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 5-30
12W deep dive: How often should a concrete mixer be cleaned, and how is the drum cleaned after a shutdown?
Clean the mixer daily if it operates continuously, or after each period of use if it operates less than 1 day. Clean the drum whenever you shut down for more than 1 1/2 hours: place a volume of coarse aggregate equal to one-half the mixer capacity in the drum, let it revolve about 5 minutes, then discharge it and flush the drum with water. Never strike the discharge chute, drum shell, or skip to remove aggregate or hardened concrete, because concrete adheres more readily to dents and bumps.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 5-31
12W deep dive: When may stiffened fresh concrete be remixed, and what limits still apply?
If concrete stiffens before the cement hydrates to its initial set, it is still usable if remixing makes it plastic enough to be compacted in the forms. Carefully add a small amount of water and remix for at least one-half of the minimum required mixing time or number of revolutions. Then test that it does not exceed the maximum allowable W/C ratio, slump, or mixing and agitating time. Do not add water randomly, because that lowers quality. Remixed concrete hardens rapidly and may cause a cold joint if fresh concrete is placed adjacent to or above it.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 5-33
12W deep dive: What are the three main requirements for transporting concrete from the plant to the job site?
Speed, so the concrete does not dry out or lose workability or plasticity between mixing and placing; minimum material segregation, to keep the mix uniform and prevent loss of fine material, cement, or water; and no delays, so placement is not interrupted by undesirable fill planes or construction joints.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 5-36
12W deep dive: What must be done before concrete is placed?
Preparation includes compacting, moistening the subgrade or placing a vapor barrier, erecting forms, and setting reinforcing steel. Moistening the subgrade is especially important in hot weather to prevent water extraction from the concrete.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), paras 5-43 and 5-44
12W deep dive: What are the principles of proper concrete placement, including the maximum free-fall drop?
Avoid segregation from the mixer to final consolidation and finishing; thoroughly consolidate the concrete around all embedded reinforcement and into all form angles and corners; obtain a good bond when placing fresh concrete against hardened concrete; and control the temperature of fresh concrete and protect it from temperature extremes after placement. Unless the free fall into the form is less than 5 feet, use vertical pipes, suitable drop chutes, or baffles.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 5-45
12W deep dive: In what order should concrete be placed in walls, beams, or girders, and how is a construction joint prepared?
Place the first batches of each layer at the ends of the section, then proceed toward the center to prevent water from collecting at the form ends and corners. For walls, overfill the form about 2 inches and remove the excess just before the concrete sets, to leave a rough, clean surface. Before placing the next lift, deposit a 1/2- to 1-inch-thick layer of sand-cement mortar made with the same water content as the concrete and a slump of about 6 inches, to prevent stone pockets and help produce a watertight joint.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 5-46
12W deep dive: How should concrete be placed in a slab, and what practices cause segregation?
Place the concrete at the far end of the slab first, then place subsequent batches against previously placed concrete. Do not place the concrete in separate piles and then level and work them together, and do not deposit it in big piles and move it horizontally to its final position. Those practices would result in segregation.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 5-47
12W deep dive: How should concrete be placed on a slope?
Always deposit the concrete at the bottom of the slope first, then proceed up the slope, placing each new batch against the previous one. When consolidated, the weight of the new concrete increases the compacting of the previously placed concrete.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 5-48
12W deep dive: Which concrete must be consolidated after placement, and what must a compacting device be able to do?
Except for concrete placed underwater, compact or consolidate all concrete after placement. Mechanical vibrators are best, but hand tools such as spades, puddling sticks, or tampers may also be used. The device must reach the bottom of the form and be small enough to pass between reinforcing bars. Work carefully around all reinforcing steel and do not displace it, because the member's strength depends on proper reinforcement location.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 5-50
12W deep dive: How is an internal vibrator used, and how long should it stay in the concrete?
Insert an internal vibrator at about 18-inch intervals—for 5 to 10 seconds in air-entrained concrete and for 10 to 15 seconds in nonair-entrained concrete. Vibrators allow placement of mixtures that are too stiff to place any other way, such as those having only a 1- or 2-inch slump.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 5-51
12W deep dive: What water temperature and current limits apply when placing concrete underwater?
For best results, do not place concrete in water whose temperature is below 45°F, nor in flowing water whose velocity is greater than 10 feet per minute, even though sacked concrete can be placed in water having greater velocities. If concrete is placed in water below 45°F, make sure the concrete temperature is above 60°F when deposited, but never above 80°F. Do not pump water while placing concrete or for 24 hours thereafter.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 5-54
12W deep dive: How does a tremie keep water and air out of concrete being placed underwater?
A tremie is a long, funnel-shaped pipe from a working platform above the water to the lowest placement point. After it is filled and lowered, the discharge end remains continually buried in newly placed concrete. Keeping the tremie constantly filled excludes both air and water from the pipe. Lift it only a little, slowly, to start the flow, taking care not to lose the seal at the discharge end.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 5-55
12W deep dive: What is screeding, and how is a screed used?
Screeding brings the surface of a floor slab, sidewalk, or pavement to the correct elevation by striking off the excess concrete. A screed is a template with a straight or curved lower edge. Move it back and forth across the concrete in a sawing motion, advancing a short distance with each motion along the form or guide strips, so excess concrete is forced into the low spots.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 5-59
12W deep dive: What are the three purposes of floating a concrete surface?
To embed aggregate particles just beneath the surface; to remove slight imperfections, high spots, and low spots; and to compact the concrete at the surface in preparation for other finishing operations. Begin floating immediately after screeding while the concrete is still plastic and workable.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 5-60
12W deep dive: Why must you not overwork plastic concrete, and when may an aluminum float be used?
Overworking plastic concrete lets an excess of water and paste rise to the surface, forming a thin weak layer that will scale or wear off under use. To avoid cracking and dusting, begin aluminum floating when the water sheen disappears from the freshly placed surface. Do not use either cement or water as an aid in finishing the surface.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 5-61
12W deep dive: When should steel troweling begin, and what happens if it is done too soon?
Begin steel troweling when the moisture film or water sheen disappears from the floated surface and the concrete has hardened enough to prevent fine material and water from working to the surface. Delay the operation as long as possible. Too much troweling too soon tends to produce crazing and reduces durability, but too long a delay makes the surface hard to finish properly. Do not spread dry cement on a wet surface to absorb excess water.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 5-62
12W deep dive: How is a nonskid broomed finish produced on concrete?
After floating, wait 10 to 15 minutes, then broom the concrete before it hardens thoroughly with a straw broom of fibers at least 4 1/2 inches long. The grooves should not be more than 3/16 inch deep. The direction of scoring should be at right angles to the direction of any traffic. When rough scoring is specified, use a stiff broom of steel wire or coarse fiber.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 5-63
12W deep dive: Why is moisture essential during curing, and what happens if the concrete dries out?
Adding water to portland cement starts hydration, which produces the hardened cement paste that holds concrete together. Both the rate and degree of hydration, and the resulting strength, depend on the curing process after placing and consolidating. Hydration continues indefinitely at a decreasing rate as long as the mixture contains water and the temperature is favorable. Once the water is removed, hydration ceases and cannot be restarted.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 5-74
12W deep dive: How long should cast-in-place concrete be cured, and at what temperature?
Curing is the period from consolidation until the concrete reaches its design strength. During this period, keep the concrete moist and as near to 73°F as practicable. For most structural use, the curing period for cast-in-place concrete is usually 3 days to 2 weeks, depending on temperature, cement type, and mix proportions. Bridge decks and other slabs exposed to weather and chemical attack usually require more extended curing periods.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 5-75
12W deep dive: What two categories of curing methods does TM 3-34.44 describe?
Methods that supply additional moisture, and methods that prevent moisture loss. They keep concrete moist and, in some cases, at a favorable hydration temperature.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 5-76
12W deep dive: How do sprinkling, wet covers, and flooding supply moisture during curing?
Sprinkling continually with water is excellent, but if you sprinkle only at intervals, do not allow the concrete to dry out between applications. Wet covers include wet burlap, cotton mats, straw, earth, and other moisture-retaining fabrics; lay them as soon as the concrete is hard enough to prevent surface damage, and keep them moist for the entire curing period. If practical, horizontal placements can be flooded by creating an earth dam around the edges and submerging the entire structure.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 5-77
12W deep dive: How is waterproof paper used to prevent moisture loss during curing?
Use waterproof paper to cure horizontal surfaces and structural concrete having relatively simple shapes. The paper should cover both the surfaces and the edges. Wet the surface with a fine water spray before covering. Lap adjacent sheets 12 inches or more and weigh their edges down to form a continuous cover with completely closed joints. Leave the coverings in place during the entire curing period.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 5-78
12W deep dive: What happens if concrete freezes shortly after placement?
Concrete that freezes shortly after placement is permanently damaged. If it freezes only once at an early age, favorable curing conditions can restore it to nearly normal, although it will neither weather as well nor be as watertight as concrete that has never frozen. Air-entrained concrete is less susceptible to freeze damage than nonair-entrained concrete. Keep the concrete at a favorable temperature until it is strong enough to withstand both low temperatures and anticipated service loads.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 5-88
12W deep dive: When may wall-form ties be removed so curing water can enter, and what caution applies in cold weather?
Ties may be removed as early as 24 hours after casting to loosen the forms slightly and permit entry of curing water between the form and the concrete. Wall forms should not be removed until the concrete has thoroughly hardened, but specified curing should begin as early as possible in warm weather. In cold weather, defer form removal or replace the form work with insulation blankets to avoid thermal shock and consequent crazing of the surface.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 5-90
12W deep dive: What is a concrete block, and what is its most common nominal size?
A concrete block is a masonry unit that is either solid or contains single or multiple hollows. Its most common unit size is 7 5/8 by 7 5/8 by 15 5/8 inches, known as 8- by 8- by 16-inch block nominal size. When laid with 3/8-inch mortar joints, the unit occupies a space exactly 8 by 8 by 16 inches.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), paras 8-1 and 8-7
12W deep dive: What are the main types of concrete masonry units, and how are load-bearing blocks graded?
The main types are hollow load-bearing concrete block, solid load-bearing concrete block, hollow nonload-bearing concrete block, concrete building tile, and concrete brick. Load-bearing blocks have two grades: Grade N for general use, including exterior walls above or below grade that may or may not be exposed to moisture or weather, and for back-up and interior walls; and Grade S for above-grade exterior walls with a weather-protective coating and for interior walls.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), paras 8-3 and 8-4
12W deep dive: How does ASTM distinguish a solid concrete block from a hollow one?
A solid concrete block has a core area not more than 25 percent of the gross cross-sectional area. A hollow concrete block has a core area greater than 25 percent—generally 40 to 50 percent. Most concrete bricks are solid.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 8-6
12W deep dive: About how much does an 8- by 8- by 16-inch hollow load-bearing block weigh?
When made with heavyweight aggregate such as sand, gravel, crushed stone, or air-cooled slag, it weighs from 40 to 50 pounds. The same type and nominal size made with lightweight aggregate such as coal cinders, expanded shale, clay, slag, volcanic cinders, or pumice weighs only 25 to 35 pounds.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 8-5
12W deep dive: How much cement should weather-exposed concrete blocks contain, and how should they be cured?
Make blocks subject to weathering with a mix of at least six sacks of cement per cubic yard of mix. Steam is the best way to cure them because it takes less time; blocks cured in wet steam at 125°F for 15 hours have 70 percent of their 28-day strength. If steam is not available, protect the blocks from the sun and keep them damp for 7 days.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), paras 8-10 and 8-11
12W deep dive: How wide should masonry wall footings be for small buildings?
Place footings on firm, undisturbed soil with adequate load-bearing capacity, and below frost penetration. Unless local requirements or codes specify otherwise, make the footings for small buildings twice as wide as the thickness of the walls they support. Footing thickness equals wall width.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 8-13
12W deep dive: How is a concrete masonry basement wall parged?
Always give exterior concrete masonry basement walls two 1/4-inch-thick coats of parging, using portland cement mortar (1:2 1/2 mix by volume) or joint mortar. In hot, dry weather, dampen the wall very lightly before the first coat. Roughen the first coat when it is partly hardened, wait 24 hours, dampen it lightly, then apply the second coat and keep it damp at least 48 hours. Do not backfill against concrete masonry walls until the first floor is in place.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 8-15
12W deep dive: What workmanship is required for weathertight concrete masonry walls?
Lay each masonry unit plumb and true. Fill both horizontal and vertical joints completely and compact them by tooling when the mortar partly stiffens. Add flashing at vertical joints in copings and caps, at joints between roofs and walls, and below cornices and other members that project beyond the wall face. Provide drips for chimney caps, sills, and other projecting ledges so water sheds away from the wall.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 8-17
12W deep dive: After the first course, how are the corners of a concrete masonry wall built up?
Build the corners next, usually four or five courses high, moving each course back one-half block. Apply mortar to the tops of the blocks already laid and to the vertical joints. Check each course at the corner with a level for alignment, level, and plumb. A story or course pole—a board with markings 8 inches apart—helps determine the top of each masonry course accurately.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 8-19
12W deep dive: How is the wall filled in between corners, and when may a block's position still be adjusted?
Stretch a mason's line along the exterior block edges from corner to corner for each course, and lay the top outside edge of each new block to this line. Tip the block slightly toward you so you can see the edge of the course below, then place it and level and align it by tapping lightly with a trowel handle. Make all final position adjustments while the mortar is soft and plastic; any adjustment after the mortar stiffens will break the mortar bond and allow water to penetrate.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 8-20
12W deep dive: How is a closure block installed, and how thick should mortar joints be?
Before installing the closure block, butter both edges of the opening and all four vertical edges of the closure block with mortar, then lower it carefully into place. The recommended width of mortar joints for concrete masonry units is about 3/8 inch. Do not spread mortar too far ahead of laying or it will stiffen and lose plasticity. Cut off excess mortar with a trowel and throw it back on the mortar board to rework into the fresh mortar; do not rework any dead mortar from the scaffold or floor.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), paras 8-21 and 8-22
12W deep dive: When and how should mortar joints in a concrete masonry wall be tooled?
After laying a section of the wall, tool the joints when the mortar becomes thumbprint hard. Tooling compacts the mortar and forces it tightly against the masonry on each side. Use either concave or V-shaped tooling. Tool vertical joints first, then strike the horizontal joints with a long jointer. Trim off mortar burrs flush with the wall face.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 8-23
12W deep dive: How are anchor bolts installed in the top of a hollow concrete masonry wall?
Place pieces of metal lath in the second horizontal mortar joint from the top, under the cores that will contain the bolts. Use 1/2-inch-diameter, 18-inch-long anchor bolts, spaced up to a maximum of 4 feet apart. After the top course is complete, insert the bolts into the cores of the top two courses and fill the cores with concrete or mortar. The threaded end should extend above the top of the wall.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 8-24
12W deep dive: What is a control joint in a masonry wall, and how is it finished if it is exposed?
Control joints are continuous vertical joints that permit the masonry wall to move slightly under unusual stresses without cracking. They are formed with a combination of full- and half-length blocks and are laid up in mortar like any other joint. If they are exposed to the weather or to view, rake the mortar out to a depth of about 3/4 inch after it is stiff, then caulk the recess.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 8-25
12W deep dive: How should intersecting concrete-block bearing walls be tied together?
Do not join them with a masonry bond except at the corners. Terminate one wall at the face of the second wall with a control joint, and tie the walls together with Z-shaped metal-tie bars 1/4 by 1 1/4 by 28 inches, with a 2-inch right-angle bend on each end. Space the tie bars no more than 4 feet apart vertically, place metal lath under the cores that will contain the ends, and embed the bends by filling those cores with mortar or concrete.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 8-28
12W deep dive: Why must mortar not be smeared into concrete-block surfaces while a wall is being laid?
Hardened, embedded mortar smears cannot be removed, even with an acid wash, and paint will not cover them. Allow droppings to dry and harden, then chip off most of the mortar with a small piece of broken concrete block or a trowel, and finish with a final brushing. Always patch mortar joints and fill holes made by nails or line pins with fresh mortar.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 8-32
12W deep dive: What is the mason responsible for when laying concrete masonry, and what does the mason's helper do?
The mason is responsible for laying out the job, keeping the walls plumb and the courses level, and the quality of detail work such as cutting and fitting masonry units, making joints, and installing anchor bolts and ties in intersecting walls. The mason's helper mixes mortar, keeps it tempered, supplies blocks and mortar, aids in layout, and sometimes lays out blocks ahead on an adjacent course.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), paras 8-33 and 8-34
12W deep dive: What is a brick, and what are the standard US brick sizes?
Bricks are small masonry units that are either solid or cored, but not more than 25 percent cored. They are kiln-fired from various clay and shale mixtures and are small enough to place with one hand. Standard US bricks are 2 1/4 by 3 3/4 by 8 inches actual size. Modular US bricks are 2 2/3 by 4 by 8 inches nominal size. English bricks are 3 by 4 1/2 by 9 inches, Roman bricks are 1 1/2 by 4 by 12 inches, and Norman bricks are 2 3/4 by 4 by 12 inches nominal size. Brick weighs from 100 to 150 pounds per cubic foot.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), paras 9-2 and 9-3
12W deep dive: What are the common cut-brick shapes and the five surfaces of a brick?
Common cut shapes are the half or bat, three-quarter closure, quarter closure, king closure, queen closure, and split. The five surfaces of a brick are the face, side, cull, end, and beds.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), paras 9-4 and 9-5
12W deep dive: What do course, wythe, stretcher, header, rowlock, and soldier mean in brick masonry?
A course is one of several continuous horizontal layers of masonry units. A wythe (sometimes called a tier) is each continuous vertical section of a wall one masonry unit thick. A stretcher is laid flat on its bed along the length of the wall with its face parallel to the wall face. A header is laid flat on its bed across the width of the wall with its face perpendicular to the wall face, generally to bond two wythes. A rowlock is a header laid on its face or edge across the width of the wall. A soldier is a brick laid on its end with its face perpendicular to the face of the wall.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 9-20
12W deep dive: What three meanings does "bond" have in masonry?
Structural bond is how the individual masonry units interlock or tie together into a single structural unit, by overlapping the units, embedding metal ties in connecting joints, or using grout to adhere adjacent wythes. Mortar bond is the adhesion of the mortar joint to the masonry units or to the reinforcing steel. Pattern bond is the pattern formed by the masonry units and mortar joints on the face of a wall; it may result from the structural bond or may be purely decorative.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 9-21
12W deep dive: What are the six basic brick bond patterns, and how do running bond and common (American) bond differ?
The six basic patterns are running bond, common or American bond, Flemish bond, English bond, stack bond, and English cross or Dutch bond. Running bond is the simplest, consisting of all stretchers and no headers, so metal ties usually form the structural bond; it is used largely in cavity walls, brick veneer, and facing-tile walls. Common or American bond is a variation of the running bond with a course of full-length headers at regular intervals, usually every fifth, sixth, or seventh course. In a common bond, use a three-quarter closure at the corner of each header course.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 9-21
12W deep dive: How are Flemish bond, English bond, and stack bond laid?
In Flemish bond, each course consists of alternating headers and stretchers, with headers in every other course centering over and under the stretchers in between. English bond consists of alternating courses of headers and stretchers; the headers center over and under the stretchers, and the joints between stretchers in stretcher courses do not align vertically. Stack bond is purely a pattern bond, with no overlapping units and all vertical joints aligning; it usually bonds to the backing with rigid steel ties, and in large or load-bearing walls steel-pencil rods are inserted into the horizontal mortar joints as reinforcement.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 9-21
12W deep dive: How does English cross (Dutch) bond differ from English bond?
English cross or Dutch bond is a variation of English bond. The only difference is that the joints between the stretchers in the stretcher courses align vertically and center on the headers in the courses above and below.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 9-21
12W deep dive: How thick should a brick mortar joint be, and why is a slush joint a poor practice?
There is no fixed rule, and irregularly shaped bricks may need joints up to 1/2 inch thick, but 1/4-inch joints are the strongest and should be used when the bricks are regular enough to permit it. A slush joint is made by depositing mortar on top of the head joints and letting it run down between the bricks; even if the space is filled, the mortar cannot be compacted against the brick faces, and a poor bond results.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), paras 9-24 and 9-25
12W deep dive: How far ahead may bed-joint mortar be spread, and how should the bed be prepared?
Do not spread the mortar for a bed joint too far ahead of laying; the length of 4 or 5 bricks is best. Mortar spread too far dries out before the bricks are bedded and causes a poor bond. The mortar must be soft and plastic. Spread it about 1 inch thick, then make a shallow furrow in it. A furrow that is too deep leaves a gap between the mortar and the bedded brick and reduces the wall's resistance to water penetration.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 9-28
12W deep dive: Why are exterior brick mortar joints finished, and what is a concave joint?
Joints are finished to make the masonry more waterproof and give it a better appearance. If joints are simply cut flush and not finished, shallow cracks develop immediately between the brick and the mortar. Always finish a joint before the mortar hardens too much. A concave joint is very weathertight; after removing excess mortar with a trowel, use a jointer slightly larger than the joint and force the mortar tight against the brick on both sides.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 9-36
12W deep dive: How are a flush joint and a weather joint made?
A flush joint is made by holding the trowel almost parallel to the face of the wall while drawing its point along the joint. A weather joint sheds water from a wall surface more easily; to make it, push downward on the mortar with the top edge of the trowel.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 9-36
12W deep dive: Which solid brick walls are the most familiar in the United States?
The solid 8- and 12-inch walls in common bond.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 9-42
12W deep dive: Should a brick be moved after it is laid in the mortar?
No. It is not good practice to move brick after it is laid in the mortar. Take great care to place the bricks accurately the first time.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 9-47
12W deep dive: How should completed brickwork be protected overnight?
Each night, cover the tops of all work completed inside the brick walls to protect them from weather damage. Use boards or tarpaulins secured by loose bricks.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 9-53
12W deep dive: How are brick-arch mortar joints made, and what temporary support is used?
Brick arches require full mortar joints. The joint width is narrower at the bottom of the arch than at its top, but it should not narrow to less than 1/4 inch at any point. As laying progresses, make sure the arch does not bulge out of position. Construct the arch over a temporary wood support called a template that remains in place until the mortar sets.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), paras 9-64 and 9-65

12W – Deep Dive: Doors, Windows, Finish Carpentry, Timber Bridges & Masonry Repair

Source: TM 3-34.47 (Carpentry, 29 Jul 2022); TM 3-34.44 (Concrete and Masonry, 23 Jul 2012 incl. C1, 2 Sep 2021). Complements earlier 12W files; does not repeat those cards. Verify current editions.

12W deep dive: How much larger than the door should a rough door opening be, and how is the opening prepared before the frame is set?
Rough openings are usually made 2 1/2 inches larger each way than the size of the door, to allow for the jambs, wedging, and clearance for the door to swing. Before the exterior covering is put on, square off uneven pieces of sheathing and wrap heavy building paper around the sides and top of the opening (not the floor, because the sill must be worked into a portion of the rough flooring).
TM 3-34.47 (29 Jul 2022), para 8-1
12W deep dive: How are doors classified, and which way should a hinged interior door not swing?
Doors, both exterior and interior, are classified as job-built or mill-built, and further as batten, panel, and flush doors. No hinged interior door should open or swing against a natural entry, swing into hallways, or be obstructed by other swinging doors.
TM 3-34.47 (29 Jul 2022), para 8-2
12W deep dive: How is a batten door made in hasty construction, and how much clearance is left when it is hung?
The carpenter makes a batten door from several 2 x 6 boards with ledgers and braces. Nail the ledgers with their edges 6 inches from the ends of the door boards, and place a diagonal board between the ledgers, beginning at the top-ledger end opposite the hinge side and running to the lower ledger. On an outside door, use roofing felt on the weather side, held by wooden laths. When these doors are hung, leave 1/4 inch of clearance around the door to allow for expansion.
TM 3-34.47 (29 Jul 2022), para 8-4
12W deep dive: What are the parts of a panel door, and how do solid-core and hollow-core flush doors differ?
Panel doors consist of vertical stiles and horizontal rails that form the framework into which panels are inserted. Additional members called muntins may divide the door into panels. Flush doors have flat surfaces on both sides. Solid-core doors have a solid particleboard or wood-block core covered with veneer; they are usually used as exterior doors, provide better sound insulation, and have less tendency to warp. Hollow-core doors have a lightweight core and are usually used as interior doors.
TM 3-34.47 (29 Jul 2022), paras 8-6 and 8-7
12W deep dive: What parts make up a door frame, and how do interior frames differ from exterior frames?
A door frame is made of the head casing, the jambs (head and two sides), and the sill (on exterior doors only). Interior door frames are made of two side jambs, a head jamb, and stop moldings that the door closes against. They have no sill and no casing; otherwise they are the same as exterior frames.
TM 3-34.47 (29 Jul 2022), paras 8-9 and 8-14
12W deep dive: Why are exterior door jambs rabbeted, and how much space should be left between the framing and the jamb?
In the type of frame shown in the TM, the door jambs are rabbeted to depths of 1/2 inch. The rabbet prevents the door from swinging through the frames; a strip of wood may be used instead of a rabbet, and the door stop also helps weatherproof the door. Door openings should allow 1/2 inch between the frame and the jamb to permit plumbing and leveling of the jambs.
TM 3-34.47 (29 Jul 2022), paras 8-10 and 8-15
12W deep dive: What stock is used for inside and outside door jambs?
Inside jambs are made of 3/4-inch stock; outside jambs are made of 1 3/8-inch stock. The width of the stock varies with the thickness of the walls. Inside jambs are built up with 3/8- x 1 3/8-inch stops nailed to the jamb. Outside jambs are usually rabbeted to receive the door.
TM 3-34.47 (29 Jul 2022), para 8-15
12W deep dive: What is the swing, or hand, of a door, and how is it determined for a standard door?
The swing describes the direction in which the door swings and from which side it is hinged. Standard doors have hinges on the left or right and swing inward. Reverse doors have hinges on the left or right and swing outward. To determine the door hand for a standard door, face the door from the hinge side; whichever hand is closer to the door knob determines whether the door is right- or left-hand.
TM 3-34.47 (29 Jul 2022), para 8-17
12W deep dive: How many hinges are used on exterior and interior doors, and which way should doors open?
Most doors are hung with the loose-pin butt hinge, so the pin can be removed and the door taken off without unscrewing the hinges. Exterior doors use three hinges to reduce warpage from different exposure on opposite sides and to support wider, heavier doors. Interior doors use two hinges. Doors should be hinged so they open in the direction of the natural entry, open out in public buildings, and swing against a blank wall whenever possible and never into a hallway.
TM 3-34.47 (29 Jul 2022), para 8-18
12W deep dive: What is a hinge gain, and what is the usual hinge setback?
The gain is the cutout or mortise made to receive a leaf of the hinge. Its depth is determined by the hinge's thickness, and its width by the hinge's size. Setback is the distance that the hinge is placed away from the side of the door, usually 3/16 inch.
TM 3-34.47 (29 Jul 2022), para 8-19
12W deep dive: What two types of locks are used in theater-of-operations construction, and what is panic hardware?
The two types are cylinder locks and tubular locks. Cylinder locks are sturdy, heavy-duty locks designed for installation in exterior doors and provide high security. Tubular locks are light-duty locks used for interior doors on bathrooms, bedrooms, passages, and closets. After the hinges are in position, mark the lock on the lock stile 36 inches from the floor. Panic hardware is another type of lock, also known as a fire-exit bolt; it is often installed on the exit doors of public buildings. Slight pressure on the touch bar retracts the latch bolts at the top and bottom.
TM 3-34.47 (29 Jul 2022), paras 8-25 and 8-26
12W deep dive: What are the most common types of windows, and what two parts does every window consist of?
The most common types are double-hung and hinged (or casement) windows. All windows consist of two parts, the frame and the sash. The sash is the framework that holds the glass. Window frames are made of four basic parts: the head, two jambs, and the sill.
TM 3-34.47 (29 Jul 2022), paras 8-27 and 8-30
12W deep dive: How does a double-hung window operate, and how may a casement window be hinged?
A double-hung window is made of upper and lower sashes that slide vertically past one another. Screens can be located on the outside of the window. Casement windows (out-swinging or in-swinging) may be hinged at the sides, top, or bottom. Casements have the advantage of catching a parallel breeze and slanting it into a room. Out-swinging casements require the screen on the inside. In-swinging casements are clear of screens but are extremely difficult to make watertight, particularly against a driving rainstorm.
TM 3-34.47 (29 Jul 2022), paras 8-28 and 8-29
12W deep dive: How much slope and overhang does a window sill usually have?
Sills have a usual slope of 1 to 5 inches so that they shed water quickly. They are wider than frames, usually extending about 1 1/2 inches beyond the sheathing.
TM 3-34.47 (29 Jul 2022), para 8-32
12W deep dive: How are sliding sashes counterbalanced?
Sliding sashes are counterbalanced by sash weights that weigh half as much as the sash. Sashes are classified as single or divided, according to the number of lights (panes of glass).
TM 3-34.47 (29 Jul 2022), para 8-34
12W deep dive: How far should a tropical hood or canopy extend from a building?
Hoods or canopies are used in tropical climates to protect the screened opening at the ends of the buildings. They are framed to the end walls with short rafters and knee braces made of 2 x 4s. The hood should extend about 2 1/2 or 3 feet from the building.
TM 3-34.47 (29 Jul 2022), para 8-42
12W deep dive: Why is sheetrock used for interior wall coverings, and in what thicknesses does it come?
In current construction, sheetrock, plywood, and fiberboard are used instead of laths and plaster. Sheetrock saves time and has a short drying time compared with plaster; it is also fire-resistant. It usually comes in sheets 4 x 8, 4 x 9, 4 x 10, 4 x 14, and 4 x 16 feet, in thicknesses of 1/4, 3/8, 1/2, or 5/8 inch.
TM 3-34.47 (29 Jul 2022), paras 9-1, 9-3, and 9-5
12W deep dive: How far apart should sheetrock nails be spaced, and how far from the edge?
If the sheetrock is single-nailed, space the nails 6 to 7 inches apart on ceilings and 6 to 8 inches apart on walls. If it is double-nailed, the centers of the nail pairs are about 12 inches apart, with each pair 2 to 2 1/2 inches apart and the outer edges 7 inches on center. The distance from the edge should be 3/8 to 1/2 inch. Do not double-nail around the perimeter of a sheet.
TM 3-34.47 (29 Jul 2022), para 9-9
12W deep dive: How should sheetrock nails be driven, and must adhesives be used alone?
Drive each nail slightly below the surface, forming a dimple, but do not break the paper. The dimple creates a pocket which is filled with joint compound. Adhesives may be used to bond single-ply sheetrock to framing, furring, masonry, insulation board, or other sheetrock, but they must be used with nails or screws.
TM 3-34.47 (29 Jul 2022), paras 9-10 and 9-11
12W deep dive: In what order should sheetrock be installed, and where should joints be avoided?
Install sheetrock on the ceiling first, then on the walls from the ceiling down to the floor. Check the layout to ensure that there will be no joints above or below door or window openings. Place each wall sheet snug against the ceiling, using a hand level to ensure that it is level, with the edges falling on the center of the studs.
TM 3-34.47 (29 Jul 2022), para 9-18
12W deep dive: How are small, fist-size, and large holes in sheetrock patched?
For small holes, apply fiber-mesh tape directly over the hole, coat it with joint compound, feather the edges, and sand or sponge the area smooth after it has dried. For fist-size holes, cut out a rectangle around the hole, glue or screw in a slightly larger backing piece, glue a patch to the backing, then tape, coat, feather, and sand. For large holes, cut a rectangular section from the centers of the nearest studs, screw or nail a patch to the studs, then tape, coat, feather, and sand.
TM 3-34.47 (29 Jul 2022), paras 9-21, 9-22, and 9-23
12W deep dive: How should baseboard and base molding be joined at corners, and how should the base shoe be nailed?
Install baseboard with a butt joint at the inside corners and a mitered joint at the outside corners, and nail it to each stud with two 8d finishing nails. Base molding should have a coped joint at inside corners and a mitered joint at outside corners. Nail the base shoe into the subfloor with long, slender nails, but not into the baseboard itself, so that a small amount of movement in the floor will not open a gap under the shoe.
TM 3-34.47 (29 Jul 2022), para 9-28
12W deep dive: What is a nonstandard fixed highway bridge, and how does a single-span bridge differ from a multispan bridge?
A nonstandard fixed highway bridge is a semipermanent bridge constructed from local materials or Class IV materials drawn from a depot. It differs from standard bridges, which are prefabricated and assembled at the site. The most common types are the simple, stringer-type (the stringers being logs) and those made of structural-grade timber or structural steel. A single-span bridge is completely supported by its two end abutments; a multispan bridge has one or more intermediate supports between the abutments. All supports of a fixed bridge transmit the load directly to the ground.
TM 3-34.47 (29 Jul 2022), paras 10-1 and 10-2
12W deep dive: What is a pile bent, and what loads and spans can it carry?
A pile bent consists of a bent cap, which provides a bearing surface for the stringers and transmits the load to the piles, and the piles, which transmit the load to the soil by tip bearing, by friction, or both. It is used for highway bridges only, is designed to carry both vertical and lateral loads, and can be used for spans of up to 50 feet.
TM 3-34.47 (29 Jul 2022), paras 10-9 and 10-10
12W deep dive: How does a trestle bent differ from a pile bent, and what are its span and height limits?
A trestle bent is like a pile bent except that posts take the place of piles. The posts transmit the load from the cap to the sill, the sill to the footings, and the footings to the soil. It is used for highway bridges only and, unlike the pile bent, is designed to carry vertical loads only. It can be used for spans of up to 30 feet and for ground-to-grade heights of up to 12 feet.
TM 3-34.47 (29 Jul 2022), paras 10-11 and 10-12
12W deep dive: What is a pile-bent pier, and what spans can it carry?
A pile-bent pier is composed of two or more pile bents with a common cap. Multiple bents give it great strength, so it can be used for both highway and railroad bridges. It will carry both vertical and lateral loads and can be used for spans of up to 200 feet. A trestle-bent pier is the same except that it has sills and footings; it is used for highway bridges only, carries vertical loads only, and can be used for spans of up to 60 feet and ground-to-grade heights of up to 18 feet.
TM 3-34.47 (29 Jul 2022), paras 10-13, 10-14, 10-15, and 10-16
12W deep dive: What is a crib pier, and what are its limits?
A crib pier is composed of logs or dimensioned timber fitted together in log-cabin style and is usually filled with rock or other stable fill material. It should be made so that it needs no exterior bracing. It is used for highway bridges only, for vertical loads only, and can be used for a span of up to 50 feet and a ground-to-grade height of up to 12 feet. As an expedient, crib piers may be built to the height of the stringers, eliminating the trestle bents.
TM 3-34.47 (29 Jul 2022), paras 10-17 and 10-18
12W deep dive: What do diaphragms do between bridge stringers, and how far apart may they be on timber stringers?
Diaphragms are braces between stringers to prevent them from deflecting laterally (buckling) under load. For timber, the ratio of the distance between diaphragms to the width of the top of the stringer (L/b) should not exceed 30. For example, diaphragms should be used every 15 feet between stringers 6 inches wide.
TM 3-34.47 (29 Jul 2022), paras 10-22 and 10-23
12W deep dive: How is a solid-plank bridge deck laid, and how is the tread placed?
For a solid-plank deck, lay planks horizontally, at right angles to the stringers, and leave a 1/4-inch space between planks to allow for swelling when wet. Extend the decking about 2 feet at approximately 5-foot intervals to support the handrail posts. The tread consists of planks, usually 2 or 3 inches thick, placed over the decking and between (but not under) the curbs, laid parallel to the direction of traffic. On one-lane bridges, the tread is limited to the path of the wheels or track; two-lane bridges are fully covered with tread.
TM 3-34.47 (29 Jul 2022), paras 10-44, 10-45, and 10-46
12W deep dive: How are curbs and handrails built on a timber-trestle bridge?
A curb system guides traffic. When assorted sizes of lumber are available, make curbs of 6- x 6-inch timber supported on 6- x 12- x 30-inch curb risers, spaced on about 5-foot centers, usually bolted to the decking with 1/2-inch bolts, two per curb riser. Handrails mark the bridge route and provide safety for pedestrians. For solid-plank decks, toenail 4 x 4 posts, or two 2 x 4s nailed together, to the extended planks. Make the posts 42 inches high and space them on 5-foot centers, so that the distance from the inside face of the curb to the inside face of the handrail is at least 10 inches.
TM 3-34.47 (29 Jul 2022), paras 10-47, 10-48, and 10-49
12W deep dive: What is a bridge end dam, and how is it built?
The end dam is the wall that withstands the earth pressure of the abutment. After the stringers and flooring are in place, construct an end dam of flooring planks across the end of the stringers. It should extend across the roadway from the top of the footing to the top of the tread.
TM 3-34.47 (29 Jul 2022), para 10-51
12W deep dive: What is a wharf, and how do bearing, fender, and mooring piles differ?
Wharf is an overall term for a waterfront structure that lets vessels lie alongside the shore for loading and unloading. Bearing piles support the wharf or pier framework and decking; they should be straight, at least 6 inches across the top and 18 inches across the butt, 60 to 80 feet long, and spaced 6 to 10 feet apart in one direction and 5 feet apart in the other. Fender piles are placed about 2 1/4 feet out from the centerline of the outside row of bearing piles and about 18 feet apart along the sides where ships dock, to absorb shock. Mooring piles are aligned with the outside row of bearing piles, spaced about 30 feet apart, and usually extend about 4 feet above the deck so mooring lines can be secured. Timber piling must be treated with creosote or another preservative to protect it from fungi and marine borers.
TM 3-34.47 (29 Jul 2022), paras 11-1, 11-3, 11-4, 11-5, and 11-6
12W deep dive: What is the carpenter's role during pile driving, and when must a pile be set back to plumb?
The equipment is operated by a special crew, but the carpenter is present during pile driving to direct the alignment of the piles. Piles should be straightened as soon as any misalignment is noticed. If a pile is more than a few inches out of plumb, it should be set true; the greater the penetration along the wrong line, the more difficult it is to get the pile back into plumb.
TM 3-34.47 (29 Jul 2022), paras 11-7 and 11-9
12W deep dive: How high should pile butts be left after driving, and how is the pile capping fastened?
Select piles so that after they are driven to the desired penetration, the butts are 2 or 3 feet higher than the desired finished elevation. Because the pile capping should bear evenly on every pile in the bent, trim accurately by nailing saw guides across all piles in the bent. After the piles are cut, place the cap, bore a hole for a driftpin through the cap into the top of each pile, and drive the driftpins. At a joint between cap timbers, bolt a splice scab across the joint to each side of the pile cap.
TM 3-34.47 (29 Jul 2022), paras 11-12 and 11-13
12W deep dive: How is standard timber-wharf decking installed?
Standard decking consists of 4- x 8-inch planks, spiked to each stringer with two 5/16- x 7-inch spikes and set with 1/4-inch spacing. Openings greater than 1/4 inch may be used between planks in areas that are subject to heavy rains.
TM 3-34.47 (29 Jul 2022), para 11-18
12W deep dive: What do fender piles do, and how are they cut off at the curb?
Timber is the most suitable material for wharf fenders in theater-of-operations construction. Fender piles cushion a wharf from the impact of ships, protect the outer row of bearing piles, and protect the hulls of craft from undue abrasion. They are not part of the structural support of the wharf, so they are easier to replace than bearing piles. They are driven at a slight batter (angle). Every third fender pile may extend 3 to 4 feet above the curb; the others are cut off flush with the top of the curb. That 3- or 4-foot extension supplements mooring hardware but is not used for warping a ship into or out of the berth.
TM 3-34.47 (29 Jul 2022), paras 11-20, 11-21, 11-22, and 11-25
12W deep dive: How soon after form removal should new concrete be repaired, and how long may wall and column forms stay in place before stripping?
When repairs are made immediately after form removal, while the concrete is quite green, the best bonds are developed. Make all repairs within 24 hours after removing forms. Recommended form-stripping time is 12 to 24 hours for walls, columns, and the sides only of beams and girders.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 5-99 and table 5-8
12W deep dive: How should a hole in new concrete be prepared and patched?
Before placing mortar or concrete into patch holes, keep the surrounding concrete wet for several hours, then brush a grout of cement and water mixed to a creamy consistency into the hole surfaces. Start curing the patch as soon as possible. Do not apply a single shallow layer of mortar on top of honeycombed concrete; instead, chip small defective areas down to solid concrete, cut the edges straight at right angles to the surface or undercut them slightly, and fill shallow holes with mortar in layers not more than 1/2 inch thick, scratching each layer to improve the bond.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), paras 5-101 and 5-102
12W deep dive: Why must feathered edges be avoided when patching a flat concrete surface?
Feathered edges around a flat patch break down. First chip an area at least 1 inch deep with edges at right angles to the surface before filling the hole. The fresh concrete should project slightly beyond the surface of the hardened concrete. Allow it to stiffen before troweling and finishing to match the adjacent surfaces.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 5-105
12W deep dive: How should old concrete be prepared for a repair, and how deep should a large repair be?
Remove all concrete of questionable quality unless nothing would be left, in which case remove only the loose material. After cleaning the cut surfaces, keep the area surrounding the repair continuously wet for several hours, preferably overnight; a good bond will not form without wetting. In large structures such as walls, piers, curbs, and slabs, the repair should be at least 6 inches deep if possible. If the old concrete contains reinforcement bars, allow a clearance of at least 1 inch around each exposed bar. Use rectangular patches and cut 1 to 2 inches vertically into the old concrete to eliminate thin or feathered edges.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), paras 5-107 and 5-108
12W deep dive: How does water usually enter a brick wall, and how can cracks between brick and mortar be reduced?
Water does not usually penetrate brick walls through the mortar or brick, but through cracks between the brick and the mortar. Cracks are more likely in head joints than in bed joints. Do not change the position of a brick after the mortar begins to set, because that destroys the bond. Wet high-suction bricks as necessary in hot weather so they do not absorb too much moisture from the mortar and cause it to shrink. Tool the exterior faces of all mortar joints to a concave finish, and completely fill all head and bed joints with mortar.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), paras 9-68 and 9-69
12W deep dive: What is parging of a brick face tier, and how are mortar-joint cracks repaired before waterproofing?
Parging, or back plastering, means plastering the back of the brick in the face tier with not less than 3/8 inch of rich cement mortar before laying the backing bricks. First cut all joints flush with the back of the face tier. Before applying waterproof or portland-cement paints, repair all cracks. To repair mortar-joint cracks, chip out the mortar around the full width of the crack to a depth of about 2 inches, scrub the hole with clean water, apply a coating of cement mortar mixed to a thick liquid while the surfaces are still wet, and then fill the hole with prehydrated mortar.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), paras 9-70 and 9-73
12W deep dive: What three ways does TM 3-34.44 list to waterproof a brick wall?
Bituminous mastic: to make a below-grade foundation wall watertight, apply two coats of bituminous mastic to the exterior brick surface. Waterproof paints: a transparent waterproof paint, such as a water solution of sodium silicate, can improve the watertightness of above-grade brick walls. Portland-cement paint generally gives excellent results if applied when the wall is at least 30 days old; dampen the surface with a water spray before applying the paint, and remove all efflorescence first.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 9-74
12W deep dive: What is fire brick used for, and how does it differ from silica brick?
Fire-resistant brick is used to line furnaces and incinerators to protect the supporting structure or outer shell from intense heat. Fire bricks are made from a special clay called fire clay, are heavier and usually larger than common brick, and have a standard size of 9 by 4 1/2 by 2 1/2 inches. Silica bricks resist acid gases, but do not use silica brick if it will be alternately heated and cooled; most incinerators should be lined with fire brick rather than silica brick.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), paras 9-75 and 9-76
12W deep dive: How should fire brick and silica brick be laid?
Fire brick requires thin mortar joints, especially in high-temperature work such as incinerators. Use a mortar of fire clay and water mixed to the consistency of thick cream. Dip the brick in the mortar, covering all surfaces except the top bed, lay it, and tap it firmly into place, making the joints as thin as possible and staggering the head joints so that bricks lap those underneath by one-half brick. Lay silica bricks without mortar, fitting them so close together that they fuse at the joints at high temperatures, and stagger the head joints the same way.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), paras 9-77, 9-78, 9-79, and 9-80
12W deep dive: How are door stops and casing installed?
When fitting doors, the stops are usually nailed in place temporarily until the door has been hung. Stops for doors in single-piece jambs are generally 1/2 inch thick and 2 inches wide, installed with a butt joint at the junction of the side and head jambs. A 45° bevel cut at the bottom of the stop, about 1 to 1 1/2 inches above the finish floor, will eliminate a dirt pocket. Casing is the trim nailed onto the jambs to finish between the jambs and the wall. Leave a margin of 1/4 inch from the edge of the jamb to the casing all around. Nail starting at the top, using 4d finishing nails along the jamb side and 6d or 8d case nails along the outer edge, and set all nailheads about 1/8 inch below the surface.
TM 3-34.47 (29 Jul 2022), paras 8-22, 8-23, and 8-24
12W deep dive: What causes "nail pops" in sheetrock, and what types of sheetrock are commonly used?
Sheetrock requires moderately low moisture content in the framing members. Drying of the members will result in nail pops, which cause the nailhead to form small humps on the surface. Gypsum board is the most commonly used wall and ceiling covering. Greenboard or blueboard is moisture resistant and is used in bathrooms, laundries, and similar areas. Foil-backed board serves as a vapor barrier on exterior walls. Backing board is used as a base sheet on multilayer applications and is not suitable for finishing and decorating. Plasterboard or gypsum lath is used for a plaster base and is not compatible with portland cement plaster.
TM 3-34.47 (29 Jul 2022), paras 9-3 and 9-4
12W deep dive: Which sheetrock thickness should be used for single-layer walls, renovations, and fire-resistant combinations?
1/4 or 3/8 inch is used effectively in renovations to cover existing finish walls with minor irregularities, but this thickness is not adequate for single-layer application. 1/2 inch is most commonly used and is adequate for studs or ceiling joists spaced 16 or 24 inches on center. 5/8 inch is widely used in multiple, fire-resistant combinations and is recommended for single-layer walls.
TM 3-34.47 (29 Jul 2022), para 9-5
12W deep dive: What are corner bead and casing bead used for on sheetrock?
The corner bead is used on all exposed (outside) corners to ensure a clean finish and to protect the outside corners of sheetrock from edge damage. It is nailed or screwed 6 inches on center to ensure that it is plumb. The casing (stop) bead is used where sheetrock sheets butt at wall intersections or wall and exposed ceiling intersections, or where otherwise specified, and is matched to the thickness of the sheetrock.
TM 3-34.47 (29 Jul 2022), paras 9-14 and 9-15
12W deep dive: What are the three main parts of a footing abutment and of a pile abutment on a timber bridge?
A footing abutment consists of footings, which transmit the load to the ground; a sill, which receives the load from the stringers and transmits it to the footings; and an end dam (or bulkhead), a wall of planks at the end of the bridge to keep the approach-road backfill from caving in between the stringers. A pile abutment has piles driven into the ground, a cap on top of the piles to receive the load from the stringers, and sheeting fastened to the piles to hold the backfill in place. On short bridges, abutment and approach preparation often require as much time as the rest of the bridge, so use the simplest abutment possible.
TM 3-34.47 (29 Jul 2022), paras 10-6, 10-7, and 10-26
12W deep dive: What three kinds of bracing are used on a nonstandard fixed timber bridge?
Bracing consists of longitudinal bracing, transverse bracing, and diaphragms. Longitudinal bracing is used to stabilize the bridge centerline. Transverse bracing provides stability at right angles to the centerline and is sometimes called sway or lateral bracing.
TM 3-34.47 (29 Jul 2022), paras 10-19, 10-20, and 10-21
12W deep dive: What logger's tools are used to move heavy timbers when building waterfront structures?
Peavy and cant hooks are lever-type tools used mainly to roll timbers. Timber carriers are two-man tools used mainly to pick up and carry timbers. Pike poles are used to hold or steady timbers while they are being placed. After the heavy timbers have been moved and placed, the carpenter's level is used to level them properly.
TM 3-34.47 (29 Jul 2022), para 11-8
12W deep dive: How is a stringpiece, or curb, installed on a timber-pile wharf?
The stringpiece (or curb) is placed on 2- x 10-inch blocking, 24 inches long, spaced on 48-inch centers along the edge of the deck. Stringpiece bolts are countersunk and the hole is seated with bituminous material. When the stringpieces are parallel to the direction of the wharf stringers, they are bolted through the blocking, the decking, and the stringer end pieces. When they are perpendicular to the stringers, they are bolted through the blocking, the decking, alternate stringers, and the pile cap.
TM 3-34.47 (29 Jul 2022), para 11-19
12W deep dive: What protective devices lengthen the life of fender piles?
A heavy timber wearing ribbon, which may easily be replaced, is sometimes installed along a line of fender piles at the elevation receiving the heaviest abrasion. Floating logs or camels (floating fenders) may be used. Rope wrappings are used particularly on corner fenders.
TM 3-34.47 (29 Jul 2022), para 11-23
12W deep dive: How should bolt holes and tie-rod holes in new concrete be filled?
When filling bolt holes, pack small amounts of mortar into place carefully. Mix the mortar as dry as possible, with just enough water to compact tightly when forced into place. Fill tie-rod holes extending through the concrete with mortar, using a pressure gun similar to an automatic grease gun.
TM 3-34.44 (23 Jul 2012 incl. C1, 2 Sep 2021), para 5-104

12W – Section floor: Electrical plan

Source: TM 3-34.47/MCRP 3-40D.3, Carpentry, 29 Jul 2022. Complements mos-12w-carpentry-masonry and mos-12w-3 through mos-12w-5. Adds a genuine electrical-plan fact; does not remake the tie-wire, timber-splice, or form-stripping cards that already sit in Electrical by keyword match. Public, unclassified sources only. Verify current editions.

12W deep dive: What does an electrical plan typically include for outlets, circuits, and lighting, and how does it relate to a floor plan?
An electrical plan is essentially a floor plan with the information required for installing electrical components and fixtures added to it. It typically includes tables and notes for a material takeoff list, general electrical notes, a legend, and other details. In the TM example, you will find outlets, the circuits they are to be placed on, and overhead lighting. Overhead lighting is often placed on a reflected ceiling plan. Carpenters may be required to adjust framing or provide blocking for some of the electrical components and fixtures, and the electrical plan gives them the information to make those determinations.
TM 3-34.47 (29 Jul 2022), para 1-19

12W – Carpentry and Masonry Specialist

Source: DA Pam 611-21 ch. 10C (Oct 2026 copy) (10-12W); DA Pam 611-21 ch. 10 MOS/skill-level classification listing (chapter-10-base); TM 3-34.47 (29 Jul 2022); TM 3-34.44 (23 Jul 2012 incl C1); TM 3-34.42 (1 Dec 2012); TC 9-524 (29 Oct 1996). Verify current editions.

12W: What is the primary role of the Carpentry and Masonry Specialist?
Status: current MOS (DA Pam 611-21 ch. 10C). To construct and repair wood, concrete, and masonry structures – buildings, bunkers, bridges, and other facilities.
DA Pam 611-21 ch. 10C (Oct 2026 copy) (10-12W) paras a and a(1)-(2)
12W: Where is 12W AIT?
Fort Leonard Wood, MO – verify current length on goarmy.com.
DA Pam 611-21 ch. 10C (Oct 2026 copy) (10-12W) para b(6) (course under the USA Engineer Center & School; ACASP alternative in b(7)); 10C gives the USAES address as Ft Leonard Wood, MO (DA Pam 611-21 ch. 10C (Oct 2026 copy) (10-12D) para a; DA Pam 611-21 ch. 10C (Oct 2026 copy) (10-12P) para b(9)). Course length not in 10C
12W: Which related engineer MOS no longer appears in the current MOS chart?
12V (Concrete and Asphalt Equipment Operator, Reserve Component) was deleted in Oct 2019 (201910) and converted to 12H, 12N and 12W.
DA Pam 611-21 ch. 10 MOS/skill-level classification listing (chapter-10-base) (12V1-3 Concrete and Asphalt Equipment Operator (RC): deletion date 201910, conversion to 12H, 12N, 12W; 21V converted to 12V in 201010)
12W: What are typical 12W tasks?
Building floor, stair, roof and wall systems; masonry walls; concrete wall and slab forms and foundations; placing concrete and doing slump tests; roof coverings, finishes, tile, doors and windows; and erecting pre-engineered buildings.
DA Pam 611-21 ch. 10C (Oct 2026 copy) (10-12W) paras a(1)-(2). Field fortifications and SWA huts were not found in 10C, TM 3-34.47 or TM 3-34.44 and were removed
12W: What is a footing?
The base of a foundation that spreads a structure's load into the soil.
TM 3-34.44 (23 Jul 2012 incl C1) para 4-45 ("Footings are installed at the base of the foundations to spread the loads over a larger ground area")
12W: What is rebar used for?
Steel reinforcing bar that adds tensile strength to concrete.
TM 3-34.44 (23 Jul 2012 incl C1) para 1-9 (members under tensile stress "must be reinforced with steel bars or mesh") and ch. 6 sec. III (reinforcing steel)
12W: What does "curing" concrete mean?
Maintaining moisture and temperature so concrete gains strength properly over time.
TM 3-34.44 (23 Jul 2012 incl C1) ch. 5 sec. IX (Curing: importance of curing to hydration; curing methods, table 5-5; figure 5-20 moist curing effect on compressive strength) and para 1-11 (surface "kept moist continuously during the curing process")
12W: What safety rules apply to power tools?
Use guards, wear eye/ear protection, inspect tools before use, and never remove safety devices.
TC 9-524 (29 Oct 1996) ch. 1, "Safety Rules for Machine Tools" (guards removed only for repair, safety glasses or goggles, ear muffs or plugs, keep power tools out of rain and wet locations); TM 3-34.42 (1 Dec 2012) figure 6-8 (jobsite checklist: "Power tools and extension cords visually inspected before use"). TM 3-34.47 has no power-tool safety section
12W: What is the skill progression for 12W?
12W has only two skill levels: 12W1O (E3/E4) and 12W2O (SGT). At skill level 3, Soldiers move to 12H Construction Engineering Supervisor (SSG, then SFC).
DA Pam 611-21 ch. 10 MOS/skill-level classification listing (chapter-10-base) (12W1-2 only; 12H3 E6, 12H4 E7); DA Pam 611-21 ch. 10C (Oct 2026 copy) (10-12H) para a(1) (12H3O performs the duties of previous skill levels in MOS 12W, 12K or 12R)
12W: How does DA Pam 611-21 summarize the 12W major duties?
The carpentry and masonry specialist performs general heavy carpentry and masonry duties. (ch. 10C)
DA Pam 611-21 ch. 10C (Oct 2026 copy) (10-12W) para a
12W: What minimum ASVAB line score does DA Pam 611-21 list for 12W?
88 in GM (General Maintenance) (ch. 10C; verify current standards).
DA Pam 611-21 ch. 10C (Oct 2026 copy) (10-12W) para b(4)(a) (GM 88; checked against 10C)
12W: What physical demands rating applies to 12W?
Moderate (Gold), with a minimum physical profile of 111221; normal color vision required (ch. 10C).
DA Pam 611-21 ch. 10C (Oct 2026 copy) (10-12W) paras b(1)-(3) (10C also requires b(5) freedom from vertigo)
12W: Under whose auspices is the 12W MOS course conducted?
The USA Engineer Center & School (DA Pam 611-21 ch. 10C).
DA Pam 611-21 ch. 10C (Oct 2026 copy) (10-12W) para b(6)
12W: What are examples of additional skill identifiers (ASIs) for 12W?
P6 – Project Management; Q6 – Protection Cell Operations (DA Pam 611-21 ch. 10C).
DA Pam 611-21 ch. 10C (Oct 2026 copy) (10-12W) para c(1)-(2)
12W: What does DA Pam 611-21 list as 12W duties at skill level 1?
Employ basic carpentry and masonry skills. Constructs floor systems, stairs, roof systems, wall systems, masonry walls, concrete wall forms, and concrete slab forms. (ch. 10C)
DA Pam 611-21 ch. 10C (Oct 2026 copy) (10-12W) para a(1) (MOSC 12W1O)

12W Carpentry and Masonry Specialist: Final exam study guide

Source: DA Pam 611-21 ch. 10C (Oct 2026 copy), 10-12W para a(1)–(2). Complements existing 12W major-duties and split SL1 and SL2 cards; does not repeat them word for word. No public STP or ICTL for 12W was on disk for this pass. No exam questions or passing scores are invented here. Public, unclassified sources only. Verify current editions.

12W (review): How do the skill level 1 carpentry and masonry tasks in DA Pam 611-21 group together?
One cluster is the building structure itself: constructing floor, stair, roof, and wall systems, masonry walls, and concrete wall and slab forms. Another is finish and install work: batter boards, suspended ceilings, exterior finishes, interior coverings, floor and wall tile, doors and windows, roof coverings, interior trim, joints and splices, pre-engineered buildings, placing concrete, identifying building materials, preparing material takeoff lists, and maintaining tools. The pamphlet also lists rescuing an electrical-shock victim among SL1 duties.
DA Pam 611-21 ch. 10C (Oct 2026 copy), 10-12W para a(1) (MOSC 12W1O). Ties the split SL1 cards in mos-12w-3.txt and mos-12w-carpentry-masonry.txt together for review.
12W (review): How do 12W duties change from skill level 1 to skill level 2 in DA Pam 611-21?
SL1 performs the basic carpentry, masonry, finishing, and electrical-shock-rescue tasks. SL2 constructs foundations and overhead forms, performs slump tests, coordinates construction planning and advises on carpentry and masonry construction, directs operational maintenance on assigned equipment, inspects carpentry and masonry components for proper installation, and ensures proper safety procedures are used.
DA Pam 611-21 ch. 10C (Oct 2026 copy), 10-12W para a(1)–(2) (MOSC 12W1O and 12W2O). Review summary only. The pamphlet’s SL2 inspection sentence is incomplete (“in accordance and ensures”); this card does not invent the missing words.

Keep going: more Engineer decks

Not your job? Use the MOS deck finder or see every MOS deck by career field.